HAYABEADS L-11 SERIES
White Cell Spacer for LCD
Features
- HAYABEADS is the best chemical stability and reliability because it is made of 100% Acrylic resin
- HAYABEADS is high performance of dispersion
- HAYABEADS can make panels with smaller number of spacers, because of its hardness
- HAYABEADS can make delicate gap controlling, because of high recoverability after compression
- HAYABEADS is high performance at high temperature and after heating
Grade
Grade | Average Diameter | Interval *** | C.V. Value | Application | Package unit |
L-11S | 4.0-7.0µm ±0.03 |
0.1µm | <=3.0% | Color-STN, FSTN DSTN, STN |
10 gram / bottle |
L-11NR * | 4.0-12.0µm ±0.05 |
0.1µm | <=4.0% | STN HTN, TN |
10 gram / bottle |
L-11R | 4.0-12.0µm ±0.05 |
0.1µm | <=4.5% | STN HTN, TN |
10 gram / bottle |
L-11TLX ** | 6.6-12.0µm ±0.05 |
0.1µm | <=4.0% | HTN, TN | 50 gram / bottle |
L-11T | 4.0-12.0µm ±0.05 |
0.1µm | <=5.0% | HTN, TN | 50 gram / bottle |
* L-11NR is the improved version of L-11R |
General Properties
Item | Data | Notes |
Specific Gravity | 1.33 | JIS K7112C |
10% Modulus of Elasticity | 65.1 kgf/mm2 | Shimazu Micro compression tester |
Refraction Index | 1.5 | Natrium Dray |
Transparency | 90% | 1 mm Plate |
Critical Surface Tension | 40 dyn/cm2 | 1 mm Plate |
Coefficient of Linear Expansion | 5 x 10-5/°C | 15 - 55°C |
Specific Resistance | 3 x 1015 Ωcm | JIS 6911 |
Surface Resistance | 1 x 1015 Ω | JIS K6911plate (1000 Hz) |
Dielectric Tangent | 0.02 | JIS K6911plate (1000 Hz) |
Water Content | 1%* | 110℃ × 1hr |
* at the shipment |
Physical Properties
Diameter | Crushing Load | Displacement | Measuring Method | |
Compression Strength and Displacement | 5.0µm | 3.7gf | 50% | Shimadzu Micro Compression Tester MCTM-200 Temperature at 20°C |
6.0µm | 4.5gf | 50% | ||
7.0µm | 6.5gf | 50% | ||
8.0µm | 9.5gf | 51% | ||
L-11 | Other Brand 1 | Other Brand 2 | ||
Diameter (µm) | 6.0 | 6.0 | 6.0 | |
10% Compression Load (gram f) | 0.26 | 0.24 | 0.18 | |
10% Modulus (kgf/mm2) | 65.1 | 59.7 | 46.0 | |
Recoverability (%) | 92.0 | 89.4 | 83.6 |
Chemical Impurity
Substance Control limit Detection Detection limit Inspection method Fe <5ppm 1ppm 0.3ppm ICP spectrophotometer Ca <5ppm <0.3ppm 0.3ppm Na <5ppm 1ppm 0.5ppm Cl <10ppm 3ppm 1ppm Ion chromatography Spraying Method
- Wet spraying
- Dry spraying